Image

Shanghai Beginor was founded in 2006, now we have 13 years experience in Silicone Potting Compound, Silicone Sealant, Epoxy Potting Compound, Epoxy Adhesive, Silicone Grease, comformal coating.

We got ISO9001, ISO14001, REACH Test Report, SGS Test Report.

Email: business@beginor-chemical.com

Image
Image

Besil 8230 is a two-component thermal conductivity silicone potting material. It has good liquidity after mixing, operation time can be adjusted according to the temperature, it can be deeply solidified at room temperature.

It is suitable for the protection of all kinds of heat dissipation and temperature resistant components, meet EU ROHS directive and SVHC REACH requirements.

· Two-component addition type silicone potting compound.

· Mix ratio is 1:1

· Low hardening shrinkage.

· Excellent high temperature electrical insulation and high stability.

· Good waterproof and moisture-proof.

· Excellent flame retardant.

 

Application:

· Automotive electronics, modules.

· LED power driver module.

· Solar module junction box.

· Electric vehicle charging column module.

· Lithium battery and capacitor bank.

· Magnetic induction coil

· power inverters

Items

Part A

Part B

Appearance

White or black sticky liquid

White sticky liquid

viscosity,cps, 25

3000±500

2500±500

Specific Gravity,g/cm3, 25℃

1.52±0.05

1.52±0.05

mixing ratio

AB = 100100

Mix viscosity,cps, 25℃

2500±500

Operating time,cps, 25℃

45±10

Tack free timecps25

80±20

Hardening conditions

25/3-5 hr or 8030mins

 

Appearance

White or black or gray, Flexible elastomer

HardnessShore A

55±5

Thermal conductivityW/mK

0. 80

Linear expansion coefficientK-1ppm

300

Dielectric strength, kV/mm, 25℃

≥20

Volume resistance ,DC 500V, Ω·CM

1.1×1015

Loss factor(1 MHz)

0.009

Dielectric constant(1 MHz)

3.00

temperature range,℃

- 60 ∽ 200

Flame resistance

V-0

 

 

 

 

 

 

Image
Image
Image

How to use:

· The glue will cause precipitation if placed too long, mix part A and part B in each package before construction.

· Weigh part A and part B by 1:1, mix well, direct injection into components (or modules). It is best to gently inject into the side of the wall to reduce the bubble formation.

· Put the encapsulated element in place for some time. After the bubble disappears, it can be heated and solidified, or solidified directly at room temperature, which requires about 4hr.

Attention of operation

· It can be improve hardening performance if remove the bubbles after mixing part A and part B.

· Seal preservation after taking part A and part B

· can lead to slow curing speed under the too low temperature and recommended workshop temperature.

·  Besil 8230 silicone potting compound is difficult to harden and contact with materials such as sulfur, amine, organic tin and unsaturated hydrocarbon plasticizer. Common substances have rosin, natural rubber, before use must be tested.

· The data of the product is tested at 25 temperature. If use in other low temperature or high temperature  

· please test.If you have any abnormality, please consult sales.

Package

· Part A: 20kg/barrel. Part B, 20kg/barrel

· Part A: 200kg/barrel. Part B, 200kg/barrel

Contact us now!

Copyrights © My Company